Figure 4From: The effect of a bonding agent and thermo-mechanical cycling on the bond strength of a glass-ceramic to gold and cobalt-chromium alloys Optical microscopic images of a Co-Cr alloy without bonding agent application (G4) after flexural bond strength test, showing opaque layer remnants on metal surface (mixed failure). Back to article page