Skip to main content

Table 8 Initial tangential Young’s modulus for the wallettes reinforced with GFRP

From: Influence of fibre reinforced polymers in the rehabilitation of damaged masonry wallettes

   Before of the reinforcement After the reinforcement
Wallettes Set up E (MPa) Average value (MPa) Variation coefficient (%) E (MPa) Average value (MPa) Variation coefficient (%)
GW1 With putty 5890 7050 12.09 6117 6837 9.81
GW2 7078 6821
GW3 Without putty 7927 6676
GW4 7306 7734