Skip to main content

Table 1 Materials used in the study

From: Influence of glass-fiber reinforcement on the flexural strength of different resin composites

Materials

Manufacturer/batch number

Chemical composition (weight  %)

Interlig

Angelus, Londrina, PR, Brazil/31464

Glass fibers—60 ± 5 %

Impregnated with 40 ± 5 % resin containing Bis-GMA, diurethane, barium glass

X-tra fil

Voco, Cuxhaven, Germany/1315355

Inorganic filler—86 %: Bis-GMA, UDMA, TEDMA

Filtek Z350 XT Flow

3M ESPE, St. Paul, MN, USA/N509855

Inorganic filler—65 %: Bis-GMA, TEGDMA, Bis-EMA

Filtek Z350 XT universal

3M ESPE, St. Paul, MN, USA/775639

Inorganic filler—78,5 %: Bis-GMA, Bis-EMA, UDMA, TEGDMA

  1. Bis-GMA bisphenylglycidyl dimethacrylate, BisEMA ethoxylated bisphenol-A dimethacrylate, TEGDMA triethylene glycol dimethacrylate, UDMA urethane dimethacrylate