Skip to main content

Table 3 Melting (Tm) and crystallization (Tc) temperatures, melting (ΔHm) and crystallization (ΔHc) heat of the powder elastomers (DSC)

From: Modifying a thermoplastic polyurethane for improving the bonding performance in an adhesive technical process

Sample name Tm (°C) Tc (°C) ΔΗm (J/g) ΔΗc (J/g)
TPU 44 18 31.0 32.1
TPU after white spirit washing 45 18 33.6 33.6
TPU after plasma treatment 44 17 35.5 35.5