Skip to main content

Table 1 Taguchi L8(27) orthogonal array, with all variables in study (size, amount and plasma surface treatment)

From: Analysis of the effect of size, amount and surface treatment on the tensile strain of a brittle adhesive reinforced with micro cork particles

Test Variable
Size (µm) Amount (%) Plasma surface treatment
1 53–38 0.25 With
2 53–38 0.25 Without
3 53–38 1 With
4 53–38 1 Without
5 125–250 0.25 With
6 125–250 0.25 Without
7 125–250 1 With
8 125–250 1 Without