From: Surface topography and bond strength of CAD–CAM milled zirconia ceramic luted onto human dentin: effect of surface treatments before and after sintering
Treatment
Moment of treatment
Before sintering
After sintering
C
0.04 ± 0.11 Aa
AO
1.79 ± 0.51 Ab
3.15 ± 1.47 Bb
GB
1.27 ± 0.65 Ab
3.37 ± 1.00 Bb
HA
1.14 ± 0.86 Ab
2.21 ± 0.55 Bb