Table 2 Push-out test failure mode distribution for each root third in the bulk-fill resin group (n = 20)

From: Bond strength of glass fiber posts cemented with bulk-fill flowable composite resin

 

Type 1

Type 2

Type 3

Type 4

Type 5

Cervical

2 (10%)

11 (55%)

1 (5%)

0 (0%)

6 (30%)

Middle

5 (25%)

5 (25%)

2 (10%)

0 (0%)

8 (40%)

Apical

2 (10%)

2 (10%)

0 (0%)

0 (0%)

16 (80%)