Skip to main content

Table 2 Manufacturing parameters and properties of reinforcing materials

From: Microbond fibre bundle pullout technique to evaluate the interfacial adhesion of polyethylene and polypropylene self reinforced composites

Property PE/PET copolymer Coated iPP fabric
Density 0.95 g/cc 0.9 g/cc
Melting point 270 °C 279 °C
Time of heating 45 min 45 min
Fiber surface Untreated Coated